Dataset of FNS Fusion Decay-Heat Benchmark

Inconel-600 (Inc600)

Z = Alloy
Form: Metallic Foil
91E−6234567891E−5234567891E−41E−51E−41E−30.010.11Min5m10mHour
FNSTotalNi57Co60mCo62mMn56V53Co62V52FNS-2000 5min Irradiation - Inc600 - TENDL-2017Time after irradiation [years]Heat Output [μW/g]
91E−6234567891E−5234567891E−4020406080100Min5m10mHour
Ni57Co60mCo62mMn56V53Co62V52FNS-2000 5min Irradiation - Inc600 - TENDL-2017Time after irradiation [years]% decay heat contribution
05101520253035404550556067890.01234567890.12345
TENDL-2017FNSFNS-2000 5min Irradiation - Inc600 - TENDL-2017Time after irradiation [minutes]Heat Output [μW/g]