Dataset of FNS Fusion Decay-Heat Benchmark

Inconel-600 (Inc600)

Z = Alloy
Form: Metallic Foil
250.01250.12511E−71E−61E−51E−41E−30.010.1DayWeek
FNSTotalCo60Co57Co58mMn56Co58Ni57FNS-1996 7hour Irradiation - Inc600 - TENDL-2017Time after irradiation [years]Heat Output [μW/g]
250.01250.1251020406080100DayWeek
Co60Co57Co58mMn56Co58Ni57FNS-1996 7hour Irradiation - Inc600 - TENDL-2017Time after irradiation [years]% decay heat contribution
05010015020025030035040045051e−3250.01250.1
TENDL-2017FNSFNS-1996 7hour Irradiation - Inc600 - TENDL-2017Time after irradiation [days]Heat Output [μW/g]